Technology of electrochemical deposition of the two-layer composite coating of the nickel-boron-diamond, iron for faceting wheels

Purpose
Production of cutting discs of type 6A2, Sp. ALN 36-142.00.000 for polishing and grinding of uncut diamonds into cut diamonds with composite coating of nickel-boron-diamond, iron

Characteristics
The technology is based on electrochemical deposition of a composite coating of nickel-boro-diamond, iron, characterized by high hardness, wear resistance and corrosion resistance


Technical characteristics of the electrolyte solution and the coating Ni-B:

Rate of coating deposition, mkm/hour 2550
Deposition temperature, °С 3040
The boron-containing compound used has high chemical resistance and efficiency coefficient  
Microhardness of the coating, Gpa 610
After heat treatment (300 °С), Gpa 1013

Advantages
  • resistance of diamond cutting discs coated with nickel-boron-diamond increases 1.3 times
  • grinding intensity increases by 30-40%
  • man-hours and materials saving is 20-30%, saving of electricity is 8-12%
  • technology of nickel-boron alloy deposition is material and resource saving